ER 1699 RS

Range
Fused cast
Subtitle

End-cast electrofused AZS (alumina-zirconia-silica) with 37% zirconia

Description

High corrosion resistance AZS for simple rectangular shapes. The very reduced casting cavity and high zirconia content increase resistance to corrosion.

Chemical and physical properties

Microstructure

Image
Microstructure of ER 1699 RS

Typical chemical composition

 
 

Typical crystallographic analysis

 
 

Physical characteristics

Description International standards British standards
Typical bulk density 3.8g/cm3 237pcf

Typical application

Specific to melting sidewall applications in flame furnaces.

Related products

Fused cast

ER 1711® RT

Void-free electrofused AZS (alumina-zirconia-silica) with 40% zirconia.

AZS material with highest corrosion resistance and good castability for various shapes and sizes. It is essentially free of casting cavities and allows a very homogeneous internal structure and corrosion resistance.

Fused cast

ER 2010 RIC RT

Void-free electrofused AZS (alumina-zirconia-silica) with 39% yttria-doped zirconia

AZS material with the highest corrosion resistance for simple rectangular shapes. The only AZS allowing joint closure at operating conditions.

Fused cast

ER 1685 RT

Void-free electrofused AZS (alumina-zirconia-silica) with 36% zirconia

High corrosion resistance AZS for simple rectangular shapes. Essentially free of casting cavity which allows a very homogeneous internal structure and corrosion resistance.

Fused cast

ER 1711® RR

End-cast electrofused AZS (alumina-zirconia-silica) with 40% zirconia

AZS material with highest corrosion resistance for simple rectangular shapes. Controlled casting cavity located at the bottom part of the block.

Monolithics

ERPLAST® 20 CEMENT

AZS sealing cement

AZS cement to seal and joint AZS surfaces.

Monolithics

ERPLAST® Z PATCH

Zircon sealing patch

Zircon mix to seal joints of mixed material including silica.